Show Hamamatsu Avalanche Photo Diode 2514028630
					
					This is all the information about APD 2514028630. If it is wrong, edit the data.
					
						
							| Subdetector specification: | 
							  | 
						
						
							| Serial: | 
							2514028630 | 
						
						
							| Type: | 
							Hamamatsu Avalanche Photo Diode | 
						
						
							| Detector: | 
							unassigned | 
						
						
							| Unit: | 
							unassigned | 
						
						
							| Preamp: | 
							0 | 
						
						
							| Current location: | 
							Bochum | 
						
						
							|   | 
							  | 
						
						
							| Installation information: | 
							  | 
						
						
							| Label: | 
							none | 
						
						
							|   | 
							  | 
						
						
							| Manufacturer information: | 
							  | 
						
						
							| Wafer position: | 
							F09 | 
						
						
							| Break-through voltage: | 
							404 V | 
						
						
							| Voltage for Gain 100 (T=+25°C): | 
							375.8 V | 
						
						
							| Dark current: | 
							5.6 nA | 
						
						
							|   | 
							  | 
						
						
							| Screening Logistics: | 
							  | 
						
						
							| Available: | 
							Yes | 
						
						
							| Storage Box: | 
							61 | 
						
						
							| Position in Box: | 
							4 | 
						
						
							| EP1 batch: | 
							36 | 
						
						
							| EP1 batch after irradiation: | 
							10126 | 
						
						
							|   | 
							  | 
						
						
							| Shipment: | 
							  | 
						
						
							| Grid number: | 
							none | 
						
						
							| Position in grid: | 
							none | 
						
						
							| Arrival for irradiation: | 
							16. Jul 2019 | 
						
						
							| Sent for analysis after irradiation: | 
							19. Jul 2019 | 
						
						
							| Return for assembly: | 
							none | 
						
						
							|   | 
							  | 
						
						
							| Irradiation: | 
							  | 
						
						
							| Date: | 
							16. Jul 2019 | 
						
						
							| Dose used: | 
							37 Gy | 
						
						
							| Temperature: | 
							20 °C | 
						
						
							| Position: | 
							none | 
						
						
							| Bias voltage: | 
							none      | 
						
						
							|   | 
							  | 
						
						
							| Annealing: | 
							  | 
						
						
							| Date: | 
							17. Jul 2019 | 
						
						
							| Temperature: | 
							80 °C | 
						
						
							| Duration: | 
							48 h | 
						
						
							|   | 
							  | 
						
						
							| Measurement results: | 
							  | 
						
						
							| Voltage for Gain 100: | 
							T = +20 °C: 375.4641494 V     T = -25 °C: 341.0024891 V | 
						
						
							| Voltage for Gain 150: | 
							T = +20 °C: 383.2452293 V     T = -25 °C: 348.2126887 V | 
						
						
							| Voltage for Gain 200: | 
							T = +20 °C: 387.5893154 V     T = -25 °C: 352.2396516 V | 
						
						
							| Gain/Voltage slope at M = 100: | 
							T = +20 °C: 4.484283714 V-1     T = -25 °C: 5.078420783 V-1 | 
						
						
							| Gain/Voltage slope at M = 150: | 
							T = +20 °C: 9.100132352 V-1     T = -25 °C: 9.892936812 V-1 | 
						
						
							| Gain/Voltage slope at M = 200: | 
							T = +20 °C: 14.35849151 V-1     T = -25 °C: 16.17564821 V-1 | 
						
						
							| Break-through voltage: | 
							T = +20 °C: 403.3134245 V     T = -25 °C: 367.3184577 V | 
						
						
							|   | 
							  | 
						
						
							| Notes: | 
							
								
							 | 
						
					
					
						
					
					Characteristics
					
						
							| Temperature | 
							Measurement | 
							Notes | 
						
						
							| No characteristics available! | 
						
					
					
						
						Upload new characteristic...
						
					
					Progression of the current during irradiation
					
						
							| Upload time | 
							Notes | 
						
						
							| No data available! | 
						
					
					
						
						Upload new progression data...
						
					
					Version history